Features
Characteristics
Electromagnetic characteristics
examples
Reference data
 
1.Composition
C Si Mn p S Cr Ni Al
-0.01% -0.20% -0.20% -0.03% -0.005% -0.2% -0.2% 7.5-8.5%

2.Mechanical property
Tensile strength (Mpa) Elongation (%) Reduction (%) Hardness (HRB)
500 34 80 80


3.Other properties
Property value
Character
Specific gravity
7.0
(Reference) Iron: 7.85
Lighter than iron by approx. 10%
Specific heat
0.143cal/gŽ
Thermal diffusion
0.0603c‡u

(Reference)

TitanF0.06505

SUS304F0.03808

Difficult to store/release heat

Thermal conductivity
0.059cal/cmsŽ
Thermal expansion
11.0~10|6i50`300ŽjA 1/Ž
Same level as iron


4.Available size
Thickness
Width

Thin sheet

-0.2‡o
-300‡o
Foil
-40ƒΚ
-150‡o
Rod
2-30
Wire rod
0.3-
0.1 is based on consultation
 
5.Workability
Workability
Weldability
Forgeability
Machine work
Press performance
TIG welding
Spot elding
Laser welding


›

(when heated)

’
’



(c)2009 c copyright GODAI all right reserved.